Causes of crushing of grinding beads
The micro glass bead, zirconium silicate bead and pure zirconium beads that are popular in the market are basically two kinds of electrofusion and sintering methods in terms of production technology. Beads form in hot air, cold air or electrolyte. If the technical parameters of a certain key are not well controlled, the following fragile beads will be produced: bubble beads, Snowman beads, tail beads, flat (Oval) beads.